Heat buildup on orbital weld head is slowing production - how do I troubleshoot this?

[Complete concern right here]"We have a group welding 6 inch OD 316L tubing with a. 109 wall density. Making use of the AMI 207 with their 7500 weld head and water cool, they are experiencing extreme heat such that production is being slowed to just 5-6 welds each day. Can you recommend some